CONCRETE BASEMENT CRACK REPAIR
- Field proven injection material
- No mess process
- Fast and inexpensive
- No drilling or chiselling required
- Area is wetted from outside to confirm location of leak
- Surface is prepared by wire brushing and cleaning area along crack
- Injection port locations are measured and marked
- Epoxy is applied and injection ports are attached to surface of crack
- Epoxy cures in about twenty minutes
- Crack is wetted from the inside through injection ports from top to bottom to confirm crack is continuous
- Urethane material is injected through ports and into cracks
- The material reacts with water to form the sealing foam
- After a curing time of aproximately two hours ports are easily snapped off and the surface is refinished